Veneering wooden door and a method for veneering an inner veneer strip of a door frame
Abstract
The present invention relates to a veneered wooden door and a method for veneering its sticking profile. Said veneered wooden door mainly comprises stiles and rails and core panels, and the stiles and rails comprise stile rail cores, edge bands and stickings. Characterizing in that the doorframe stickings are made of ordinary wood or artificial board instead of high grade wood, with its outer part veneered with high grade wood veneers. The method for veneering the sticking profile of the wooden door comprising the following steps: applying resin glue on backside of a high-grade wood veneer, pasting it on the surface of the stickings, then putting the wooden door into a tamping machine, with the temperature adjusted to 60˜120° C., and the pressure to 5˜15 kg/cm, applying the pressure for 2˜3 minutes.
Claims
exact text as granted — not AI-modified1 . A kind of veneered wooden doors, mainly comprises stiles and rails and core panels, wherein the stiles and rails comprise stile rail cores, edge bands and stickings, wherein the stile rail cores are made of wood of ordinary trees or artificial boards, the edge bands are made of high quality wood, the core panels are made of wood of ordinary trees or artificial boards, and the outer part of the core panels are veneered with high quality veneers, characterized that the high quality wood used in the stickings is replaced with ordinary wood or artificial boards, and the sticking profile is veneered with wood veneers containing high quality wood grains.
2 . The veneered wooden doors as described in claim 1 , wherein the stickings and the stile rail cores are made of same wood or artificial boards, and are made as a whole.
3 . A method for veneering sticking profile of a wooden door, comprising the steps of: applying resin glue on one side of a high-grade wood veneer, pasting it on the surface of the stickings of the wooden door; then putting the wooden door into a tamping machine having the same shape as the irregular surface of the sticking profile, with the temperature adjusted to 60˜120° C., and the pressure to 5˜15 kg/cm, applying the pressure for 2˜3 minutes.
4 . The veneered wooden doors as described in claim 1 , wherein the stickings and the stile rail cores are made of different wood or artificial boards.Join the waitlist — get patent alerts