US2006168800A1PendingUtilityA1

Non-Aqueous Electrolyte Secondary Battery and Method of Manufacturing the Same

Assignee: MATSUSHITA ELECTRIC INDUSTRIAL CO LTDPriority: Jul 23, 2001Filed: Apr 13, 2006Published: Aug 3, 2006
Est. expiryJul 23, 2021(expired)· nominal 20-yr term from priority
Y02P70/50H01M 10/052H01M 4/131H01M 10/0565H01M 50/1245H01M 4/13H01M 10/0585H01M 50/124H01M 10/526H01M 10/0587H01M 10/0525H01M 10/058H01M 10/52H01M 4/133H01M 4/525Y10T29/49108Y02E60/10Y10T29/49115
54
PatentIndex Score
0
Cited by
0
References
0
Claims

Abstract

A non-aqueous electrolyte secondary battery has an electrode plate assembly including a positive electrode, a negative electrode, and a separator interposed between the positive electrode and the negative electrode; a non-aqueous electrolyte including a lithium salt and a non-aqueous solvent; and a gas absorbing element that absorbs gas produced in the secondary battery, wetting of the gas absorbing element with the non-aqueous solvent is controlled.

Claims

exact text as granted — not AI-modified
1 - 7 . (canceled)  
   
   
       8 . A method of manufacturing a non-aqueous electrolyte secondary battery, comprising the steps of: 
 (1) heating a carbon powder in an inert atmosphere at 600 to 1300° C. for 10 to 120 minutes to prepare a gas absorbent comprising a simple substance of carbon, said gas absorbent capable of selectively absorbing at least one selected from the group consisting of carbon dioxide and methane;    (2) preparing an electrode material mixture including said gas absorbent and an electrode active material and applying said electrode material mixture on a collector to obtain an electrode; and    (3) assembling said electrode, a separator, and a non-aqueous electrolyte to a non-aqueous electrolyte secondary battery.    
   
   
       9 . The method of manufacturing a non-aqueous electrolyte secondary battery in accordance with  claim 8 , wherein said powdery carbon material is at least one selected from the group consisting of carbon black and active carbon.  
   
   
       10 . The method of manufacturing a non-aqueous electrolyte secondary battery in accordance with  claim 8 , wherein said powdery carbon material has a specific surface area of 50 to 1500 m 2 /g.