US2009064819A1PendingUtilityA1

Fe-based sintered alloy

Assignee: ANDO KIMIHIKOPriority: Apr 22, 2005Filed: Mar 17, 2006Published: Mar 12, 2009
Est. expiryApr 22, 2025(expired)· nominal 20-yr term from priority
C22C 33/0271C22C 33/0278C22C 38/02
40
PatentIndex Score
0
Cited by
0
References
0
Claims

Abstract

There is here disclosed an Fe-based sintered alloy produced through a mixing step of mixing an Fe—Mn alloy powder, graphite powder and Fe powder by a mixer (S 16 ), a compacting step of compacting the mixed powder at a predetermined pressure (S 18 ), and a sintering step of sintering the resultant compact in a sintering oven at a predetermined temperature for a predetermined time (S 20 ), the Fe—Mn alloy powder being characterized by containing 2-30 mass % of Mn. In particular, the mixing step (S 16 ) is carried out by mixing 5-50 mass % of the Fe—Mn alloy powder, 0.2-2 mass % of the graphite powder, and the remainder of the Fe powder in the mixer. Consequently, mechanical strength of the Fe-based sintered alloy can be further improved.

Claims

exact text as granted — not AI-modified
1 . An Fe-based sintered alloy produced through
 a mixing step of mixing an Fe—Mn alloy powder, graphite powder and Fe powder,   a compacting step of compacting the mixed powder, and   a sintering step of sintering the resultant compact,   the Fe—Mn alloy powder being characterized by containing 2-30 mass % of Mn.   
     
     
         2 . The Fe-based sintered alloy according to  claim 1 , wherein the mixing step is characterized by mixing 5-50 mass % of the Fe—Mn alloy powder, 0.2-2 mass % of the graphite powder, and the remainder of the Fe powder.