US2009162753A1PendingUtilityA1
Spherical carbons and method for preparing the same
Est. expiryApr 17, 2021(expired)· nominal 20-yr term from priority
H01M 10/052H01M 4/583C01P 2006/12H01M 4/133C01B 32/05C01B 32/205C01P 2004/32C01P 2004/61C01B 32/20Y02E60/10
61
PatentIndex Score
0
Cited by
0
References
0
Claims
Abstract
The present invention provides a method for preparing spherical carbon comprising step of heat-treating a mixture of a carbon precursor and dispersion media, a spherical non-graphitizable carbon using the same, and a method for preparing spherical artificial graphite.
Claims
exact text as granted — not AI-modified1 . A battery comprising the spherical non-graphitizable carbon comprising 10 wt % or more of spherical particles satisfying the following Mathematical Formula 1:
0.99≦a/b≦1 [Mathematical Formula 1]
where a is a minor axis of a particle and b is a major axis of a particle.
2 . The battery according to claim 1 , wherein the remaining particles of the spherical non-graphitizable carbon satisfy the following Mathematical Formula 2:
0.1≦a/b<0.99 [Mathematical Formula 2]
where a is a minor axis of a particle and b is a major axis of a particle.)
3 . The battery according to claim 1 , comprising a cathode, an anode, an electrolyte, and a separator inserted between the anode and the cathode, wherein the anode comprises the spherical non-graphitizable carbon.
4 . The battery according to claim 1 , wherein the average particle diameter of the spherical non-graphitizable carbon is 1 to 40 μm.
5 . The battery according to claim 1 , wherein the specific surface area of the spherical non-graphitizable carbon is 3 m 2 /g or less.Join the waitlist — get patent alerts
Track US2009162753A1 — get alerts on status changes and closely related new filings.
We store only your email — no account needed. See our privacy policy.