US2011178234A1PendingUtilityA1

Water-based resin compositon and articles made therefrom

Assignee: ALLEGIANCE CORPPriority: Mar 14, 2008Filed: Mar 31, 2011Published: Jul 21, 2011
Est. expiryMar 14, 2028(~1.6 yrs left)· nominal 20-yr term from priority
C08J 2309/00C08J 3/05C08K 5/0008C08C 1/075C08L 9/10C08J 3/07
61
PatentIndex Score
0
Cited by
0
References
0
Claims

Abstract

An aqueous elastomer dispersion includes a dispersed phase and an aqueous phase. The dispersed phase includes an elastomer including curable aliphatic conjugated-diene elastomers, such as polyisoprene, and a minor amount of at least one additive. The aqueous phase includes water and other optional components in either a soluble state or a dispersion state. The aqueous elastomer dispersion may be prepared by dissolving an elastomer, such as rubber, and additives in a solvent mixture and then converting the resulting solution into an aqueous emulsion. The aqueous emulsion is concentrated and the solvent is stripped from it to yield a dilute latex. The dilute latex that is obtained is concentrated again. Articles made from the aqueous elastomer dispersion include medical gloves, condoms, probe covers, dental dams, finger cots, catheters and the like.

Claims

exact text as granted — not AI-modified
1 . A method of preparing an aqueous elastomer dispersion, comprising the steps of:
 preparing an elastomer/additive solution comprising an elastomer, at least one additive, and a solvent system;   emulsifying the elastomer/additive solution to form an emulsion;   concentrating the emulsion to form a concentrated emulsion;   removing substantially all of the solvent system from the concentrated emulsion to form a substantially solvent-free dispersion; and   optionally concentrating the substantially solvent-free dispersion.   
     
     
         2 . The method of  claim 1 , wherein the elastomer is selected from the group consisting of polyisoprene, polychloroprene, styrene-butadiene copolymers, acrylonitrile-butadiene copolymers, styrene block copolymers, and butyl rubber. 
     
     
         3 . The method of  claim 2 , wherein the elastomer has a molecular weight of about 100,000 to about 3,000,000. 
     
     
         4 . The method of  claim 2 , wherein the at least one additive is selected from the group consisting of sulfur/sulfur donors, peroxide curing/crosslinking agents, vulcanization accelerators, vulcanization activators, antioxidants, stabilizers, plasticizers, antiozonants, pigments, fillers, antimicrobial agents, indicators, and additional polymers. 
     
     
         5 . The method of  claim 4 , wherein an amount of the at least one additive is about 0.5-49% by weight of total solids of the aqueous elastomer dispersion. 
     
     
         6 . The method of  claim 1 , wherein the solvent system includes a first solvent and second solvent. 
     
     
         7 . The method of  claim 6 , wherein the elastomer is soluble in the first solvent, and the at least one additive is soluble in the second solvent. 
     
     
         8 . The method of  claim 6 , wherein the first solvent includes one or more solvents, and the second solvent includes one or more solvents. 
     
     
         9 . The method of  claim 1 , wherein the emulsifying step comprises adding an emulsifier. 
     
     
         10 . The method of  claim 9 , wherein the emulsifying step further comprises mixing with a high shear mixer. 
     
     
         11 . The method of  claim 1 , wherein one or both of the concentrating steps comprise adding a creaming agent. 
     
     
         12 . The method of  claim 11 , wherein one or both of the concentrating steps further comprise separating a concentrate and an aqueous solution. 
     
     
         13 . The method of  claim 1 , wherein one or both of the concentrating steps is carried out by centrifuging using a continuous centrifugal separator. 
     
     
         14 . The method of  claim 1 , wherein the removing step comprises evaporating the solvent system from the concentrated solution. 
     
     
         15 . The method of  claim 1 , wherein the removing step comprises heating the concentrated solution to evaporate the solvent system. 
     
     
         16 . The method of  claim 1 , further comprising the step of adjusting the pH of the aqueous elastomer dispersion. 
     
     
         17 . The method of  claim 1 , wherein the total solids content of the aqueous elastomer dispersion is about 45-65% by weight. 
     
     
         18 . The method of  claim 1 , further comprising the step of making an article from the aqueous elastomer dispersion. 
     
     
         19 . The method of  claim 18 , wherein the article is selected from the group consisting of gloves, condoms, probe covers, dental dams, finger cots, and catheters.