US2012177865A1PendingUtilityA1
Reinforced polystyrene board
Est. expirySep 29, 2029(~3.2 yrs left)· nominal 20-yr term from priority
B32B 13/045B32B 2262/101B32B 2307/54B32B 2262/106B32B 2266/0228E04C 2/22B32B 5/028B32B 2307/714Y10T428/23B32B 15/02B32B 2307/546B32B 5/245E04B 1/762B32B 2307/304E04B 1/80B32B 2262/103B32B 2607/00
41
PatentIndex Score
0
Cited by
0
References
0
Claims
Abstract
A reinforced polystyrene board, includes a grid reinforcer arranged in a board surface of a polystyrene board, so as to improve a tensile strength and a folding strength of the polystyrene board, and the grid reinforcer is made of a glass fiber grid, a metal grid, or a man-made fibers grid. A protective layer of the polystyrene board arranged outside of the reinforcer isolates the reinforcer from an external environment, so as to improve the corrosion resistance and the durability of the reinforcer.
Claims
exact text as granted — not AI-modified1 - 19 . (canceled)
10 . A reinforced polystyrene board, which is an thermal insulation polystyrene laminate consisting of a polystyrene laminate and a two-dimensional grid reinforcer layer disposed in a surface layer of the polystyrene laminate, wherein a polystyrene laminate protective layer is disposed on an outer surface of said two-dimensional grid reinforcer, and by using a method that accomplishes compression molding said grid reinforcer and said polystyrene laminate at a time, said grid reinforcer is disposed in said surface layer of said polystyrene laminate.
11 . The reinforced polystyrene board as recited in claim 10 , wherein said reinforcer is formed by knitting decussations of man-made fibers warps and wefts, and a distance between the grid apertures of the man-made fibers grid reinforcer is 5×5˜20×20 mm.
12 . The reinforced polystyrene board as recited in claim 10 , wherein a thickness of said polystyrene laminate protective layer is 5˜15 mm; said polystyrene laminate protective layer and said polystyrene core laminate form an integral laminate.
13 . The reinforced polystyrene board as recited in claim 10 , wherein said man-made fibers grid is formed by knitting decussations of man-made fibers warps and man-made fibers wefts, an optimal distance between said grid apertures is 10×10˜15×15 mm.
14 . The reinforced polystyrene board as recited in claim 10 , wherein an optimal thickness of said polystyrene laminate protective layer is 8˜12 mm; said polystyrene laminate protective layer and said polystyrene core laminate form an integral laminate.
15 . A metal grid reinforced polystyrene board, which is an thermal insulation polystyrene laminate consisting of a polystyrene laminate and a two-dimensional metal grid reinforcer disposed in a surface layer of said polystyrene laminate, wherein a polystyrene laminate protective layer is disposed on an outer surface of said two-dimensional grid reinforcer, and by using a method that accomplishes compression molding said grid reinforcer and said polystyrene laminate at a time, said grid reinforcer is disposed in said surface layer of said polystyrene laminate.
16 . The metal grid reinforced polystyrene board as recited in claim 15 , wherein a metal fiber grid reinforcer is formed by electric welding decussations of longitudinal steel wires and transverse steel wires, a distance between the grid apertures of said metal fiber grid reinforcer is 5˜60×5˜60 mm, said metal fiber grid reinforcer is a hot-galvanized steel wire, a cold drawn low carbon steel wire, a stainless steel wire or an alloy steel wire, and a diameter of the steel wire is 0.5˜4.0 mm.
17 . The metal grid reinforced polystyrene board as recited in claim 15 , wherein a thickness of said polystyrene laminate protective layer is 5˜50 mm; said polystyrene laminate protective layer and said polystyrene core laminate form an integral laminate.
18 . The metal grid reinforced polystyrene board as recited in claim 15 , wherein said reinforcer is formed by electric welding decussations of longitudinal steel wires and transverse steel wires, an optimal distance between said grid apertures of said metal fiber grid reinforcer is 10˜30×10˜30 mm, and said metal fiber grid reinforcer is hot-galvanized steel wire, cold drawn low carbon steel wire, stainless steel wire or alloy steel wire, an optimal diameter of said steel wire is 0.9˜2.5 mm.
19 . The metal grid reinforced polystyrene board as recited in claim 15 , wherein an optimal thickness said protective layer of said reinforced polystyrene board is 8˜30 mm; and said polystyrene laminate protective layer and said polystyrene core laminate form an integral laminate.
20 . A glass fiber grid reinforced polystyrene board, which is an thermal insulation polystyrene laminate consisting of a polystyrene laminate and a two-dimensional glass grid reinforcer disposed in a surface layer of said polystyrene laminate, wherein a polystyrene laminate protective layer is disposed on an outer surface of said two-dimensional grid reinforcer, and by using a method that accomplishes compression molding said grid reinforcer and said polystyrene laminate at a time, said grid reinforcer is disposed in said surface layer of said polystyrene laminate.
21 . The glass fiber grid reinforced polystyrene board as recited in claim 20 , wherein said reinforcer is formed by knitting decussations of a man-made fibers warps and wefts, and a distance between the grid apertures of the man-made fibers grid reinforcer is 5˜25×5˜25 mm; a glass fiber grid reinforcer is disposed in double sides or single side of the polystyrene laminate.
22 . The glass fiber grid reinforced polystyrene board as recited in claim 20 , wherein a thickness of said polystyrene laminate protective layer is 5˜15 mm; said polystyrene laminate protective layer and said polystyrene core laminate form an integral laminate.
23 . The glass fiber grid reinforced polystyrene board as recited in claim 20 , wherein said reinforcer is formed by knitting decussations of a man-made fibers warps and wefts, an optimal distance between the grid apertures of the man-made fibers grid reinforcer is 7˜15×7˜15 mm; said reinforcer is disposed in double sides or single side of said polystyrene laminate.