US2012263623A1PendingUtilityA1

Titanium aluminide based alloy

Assignee: OEHRING MICHAELPriority: Nov 23, 2004Filed: Jun 28, 2012Published: Oct 18, 2012
Est. expiryNov 23, 2024(expired)· nominal 20-yr term from priority
C22C 14/00B22D 21/005
50
PatentIndex Score
0
Cited by
0
References
0
Claims

Abstract

The invention concerns alloys made through the use of melting and powdered metallurgical techniques on the basis of titanium aluminides with an alloy composition of Ti-z Al-y Nb where 44.5 Atom % ≦z≦47 Atom %, 44.5 Atom % ≦z≦45.5 Atom %, and 5 Atom % ≦y≦10 Atom % with possibly the addition of B and/or C at a content between 0.05 Atom % and 0.8 Atom %. Said alloy is characterized in that it contains a molybdenum (Mo) content ranging between 0.1 Atom % to 3.0 Atom %.

Claims

exact text as granted — not AI-modified
1 . An alloy made on the basis of titanium aluminide through the use of melting and powdered metallurgical techniques the alloy comprising Ti-z Al-y Nb where 44.5 Atom % is ≦z≦47 Atom %, and where 5 Atom % is ≦y≦10 Atom %, and the alloy containing molybdenum (Mo) in between 0.1 Atom % to 3 Atom % and defining a β-phase present up to a temperature of about 1,320 degrees C. 
     
     
         2 . An alloy as defined by  claim 1  wherein 44.5 Atom % is ≦z≦45.5 Atom %. 
     
     
         3 . An alloy on the basis of titanium aluminide made with the use of melting and powdered metallurgical techniques the alloy comprising Ti-z Al-y Nb-x B where 44.5 Atom % is ≦z≦47 Atom % and where 5 Atom % is ≦y≦10 Atom % and 0.05 Atom % is ≦x≦0.8 Atom % and wherein the alloy contains molybdenum (Mo) between 0.1 Atom % to 3 Atom % and defining a β-phase present up to a temperature of about 1,320 degrees C. 
     
     
         4 . An alloy as defined by  claim 3  wherein 44.5 Atom % is ≦z≦45.5 Atom %. 
     
     
         5 . An alloy on the basis of titanium aluminide made with the use of melting and powdered metallurgical techniques the alloy comprising Ti-z Al-y Nb-w C where 44.5 Atom % is ≦z≦47 Atom %, and where 5 Atom % is ≦y≦10 Atom % and 0.05 Atom % is ≦w≦0.8 Atom %, and wherein the alloy contains molybdenum (Mo) between 0.1 Atom % to 3 Atom % and defining a β-phase present up to a temperature of about 1,320 degrees C. 
     
     
         6 . An alloy as defined by  claim 5  wherein 44.5 Atom % is ≦z≦45.5 Atom %. 
     
     
         7 . An alloy as defined by  claim 5  wherein the alloy contains molybdenum between 0.5 Atom % to 3 Atom %. 
     
     
         8 . An alloy on the basis of titanium aluminide made with the use of melting and powdered metallurgical techniques the alloy comprising Ti-z Al-y Nb-x B-w C where 44.5 Atom % is ≦z≦47 Atom %, and where 5 Atom % is ≦y≦10 Atom % and 0.05 Atom % is ≦x≦0.8 Atom % and 0.05 Atom % is ≦w≦0.8 Atom %, and wherein the alloy contains molybdenum (Mo) between 0.1 Atom % to 3 Atom % and defining a β-phase present up to a temperature of about 1,320 degrees C. 
     
     
         9 . An alloy as defined by  claim 8  wherein 44.5 Atom % ≦z≦45.5 Atom %. 
     
     
         10 . A construction component made from an alloy according to  claim 1 . 
     
     
         11 . A construction component made from an alloy according to  claim 3 . 
     
     
         12 . A construction component made from an alloy according to  claim 5 . 
     
     
         13 . A construction component made from an alloy according to  claim 8 .