US2013059145A1PendingUtilityA1

Method for making polyurethane foam floor covering products with postconsumer carpet fibers

48
Assignee: JENKINES RANDALL CPriority: Jun 15, 2010Filed: May 19, 2011Published: Mar 7, 2013
Est. expiryJun 15, 2030(~3.9 yrs left)· nominal 20-yr term from priority
D06N 3/0002Y10T428/249953D06N 2211/066D06N 3/0043D06N 2205/18B29K 2105/128D06N 2205/04B29C 44/332B29L 2031/732B29C 44/569B29K 2075/00D06N 3/14B32B 5/18Y02P70/62
48
PatentIndex Score
0
Cited by
0
References
0
Claims

Abstract

Polyurethane floor covering products are formed from a web layer containing at least 30% by weight fibers. A cooled polyurethane foam formulation which includes at least one polyisocyanate, water and at least one polyol having an equivalent weight of at least 500 is applied to the web layer. The wetted web layer is then compressed to mechanically wet out the fibers, gauged and heated to cure the foam formulation.

Claims

exact text as granted — not AI-modified
1 . A process for preparing a foamed polyurethane floor covering product, comprising:
 a) forming a web layer containing at least 30% by weight fibers, such that the web layer has a weight of from 150 to 660 g/m 2  and the fibers in the web layer have an average length of from 0.75 to 40 cm;   b) continuously applying a cooled polyurethane foam formulation which includes at least one polyisocyanate, water and at least one polyol having an equivalent weight of at least 500 to the web layer, the cooled polyurethane foam formulation having a temperature of no more than 15° C. when applied to the web layer, and compressing the web layer and applied polyurethane foam formulation together to mechanically wet out the fibers in the web layer; and then   c) gauging the wetted web layer to a thickness of from 0.25 to 1.0 inches and, while maintaining the gauge, heating the polyurethane foam formulation to a temperature of from 80 to 160° C. to cure the polyurethane foam formulation to produce a cured and gauged polyurethane foam cushion containing from 5 to 50% by weight of the fibers.   
     
     
         2 . The process of  claim 1 , wherein the cooled polyurethane foam formulation has a temperature of not more than 10° C. when applied to the web layer. 
     
     
         3 . The process of  claim 1 , wherein the web layer contains at least 50% by weight of fibers. 
     
     
         4 . The process of  claim 1 , wherein the web layer further contains at least 50% by weight of fibers. 
     
     
         5 . The process of  claim 1 , wherein the web layer comprises carded fibers. 
     
     
         6 . The process of  claim 1 , wherein the fibers are obtained from postconsumer carpeting products. 
     
     
         7 . The process of  claim 1 , wherein the foamed polyurethane floor covering product has a density of from 3 to 10 pounds/cubic foot (48-160 kg/m 3 ). 
     
     
         8 . A foamed polyurethane floor covering product produced by the process of  claim 1 . 
     
     
         9 . The product of  claim 8  which contains from 5 to 30% of fibers.