Abstract
A plug for hot tube-making having a sprayed coating resistant to peeling is provided. A method for producing a plug for hot tube-making according to the present embodiment includes a step of preparing a plug whose surface includes a sprayed coating formed thereon, the sprayed coating containing iron and an iron oxide; and a heat treatment step during which the plug is kept at 400° C. to 550° C. for 5 to 60 minutes.
Claims
exact text as granted — not AI-modified1 . A method for producing a plug for hot tube-making, comprising
a step of preparing a plug whose surface includes a sprayed coating formed thereon, the sprayed coating containing iron and an iron oxide; and a heat treatment step during which the plug is kept at 400° C. to 550° C. for 5 to 60 minutes.
2 . The method for producing a plug according to claim 1 , wherein
the step of preparing the plug further comprises: a step of preparing a plug body; and a step of forming the sprayed coating by performing arc spraying with an iron wire rod onto a surface of the plug body.Join the waitlist — get patent alerts