US2019153228A1PendingUtilityA1

Use of a wax-modified, air rectified asphalt in built up roofing asphalt compositions

51
Assignee: OWENS CORNING INTELLECTUAL CAPITAL LLCPriority: Nov 21, 2014Filed: Jan 17, 2019Published: May 23, 2019
Est. expiryNov 21, 2034(~8.4 yrs left)· nominal 20-yr term from priority
E04D 11/02C08L 91/06C08L 95/00E04D 7/00C08L 2555/72C08L 2555/64C08L 2201/08
51
PatentIndex Score
0
Cited by
0
References
0
Claims

Abstract

A composition and method for making a heat stable, low application temperature Built Up Roofing Asphalt (BURA) is provided. The composition comprises a wax-modified, air rectified asphalt conforming to Type 3 BURA and, in some embodiments, Type 4 BURA specifications.

Claims

exact text as granted — not AI-modified
1 - 13 . (canceled) 
     
     
         14 . An asphalt composition comprising:
 an air rectified asphalt blown to a first softening point from about 140° F. to about 175° F.; and   a wax additive, wherein the additive has a melt point higher than about 100° C.;   wherein the asphalt composition has a penetration at 25° C. of 12 dmm to 35 dmm.   
     
     
         15 . The asphalt composition of  claim 14 , wherein the asphalt composition has an equiviscous temperature (EVT) of from about 340° F. to about 390° F. for mopping applications and from about 380° F. to about 430° F. for mechanical applications. 
     
     
         16 . The asphalt composition of  claim 14 , wherein the air rectified asphalt is blown to a first softening point that is at least about 145° F. 
     
     
         17 . The asphalt composition of  claim 14 , wherein the air rectified asphalt is blown to a first softening point from about 145° F. to about 165° F. 
     
     
         18 . The asphalt composition of  claim 14 , wherein the air rectified asphalt is blown to a first softening point that is at least about 156° F. 
     
     
         19 . The asphalt composition of  claim 14 , wherein the air rectified asphalt is blown to a first softening point of about 164° F. 
     
     
         20 . The asphalt composition of  claim 14 , wherein the wax additive comprises from about 1.5% to about 4.5% based on the weight of the total asphalt composition. 
     
     
         21 . The asphalt composition of  claim 14 , wherein the wax additive comprises one or more of a functionalized wax, a synthetic wax, or a naturally occurring wax. 
     
     
         22 . The asphalt composition of  claim 14 , wherein the wax additive comprises a synthetic wax selected from ethylene bis-stearamide wax (EBS), Fischer-Tropsch wax (FT), oxidized Fischer-Tropsch wax (FTO), polyolefin wax, polyethylene wax (PE), oxidized polyethylene wax (PEO), polypropylene wax, polypropylene/polyethylene wax, alcohol wax, silicone wax, petroleum wax, microcrystalline wax, or paraffin. 
     
     
         23 . The asphalt composition of  claim 22 , wherein the wax additive comprises one or more of a Fischer-Tropsch wax, a polyethylene wax, and an ethylene bis-stearamide wax. 
     
     
         24 . The asphalt composition of  claim 14 , wherein the wax additive comprises a functionalized wax selected from amine waxes, amide waxes, ester waxes, carboxylic acid waxes, and microcrystalline waxes. 
     
     
         25 . The asphalt composition of  claim 14 , wherein the wax additive comprises a naturally occurring wax derived from a plant, animal or mineral. 
     
     
         26 . The asphalt composition of  claim 25 , wherein the naturally occurring wax is selected from candelilla wax, carnauba wax, rice wax, Japan wax, jojoba oil, beeswax, lanolin whale wax, montan wax, ozokerite and ceresin. 
     
     
         27 . The asphalt composition of  claim 14 , wherein the asphalt composition has a minimum solubility in trichloroethylene of 99%. 
     
     
         28 . The asphalt composition of  claim 14 , wherein the asphalt composition has a penetration at 25° C. of 15 dmm to 35 dmm. 
     
     
         29 . The asphalt composition of  claim 14 , wherein the asphalt composition has a penetration at 25° C. of 12 dmm to 25 dmm. 
     
     
         30 . An asphalt composition comprising:
 an air rectified asphalt; and   a wax additive, wherein the additive has a melt point higher than about 100° C.;   wherein the asphalt composition has an equiviscous temperature (EVT) of from about 340° F. to about 390° F. for mopping applications and from about 380° F. to about 430° F. for mechanical applications.   
     
     
         31 . The asphalt composition of  claim 30 , wherein the air rectified asphalt is blown to a first softening point from about 140° F. to about 175° F. 
     
     
         32 . The asphalt composition of  claim 30 , wherein the air rectified asphalt does not include a blowing catalyst. 
     
     
         33 . The asphalt composition of  claim 30 , wherein the asphalt composition has a penetration at 25° C. of 12 dmm to 35 dmm.