US2019160523A1PendingUtilityA1

Water-cooled mold for casting aluminum alloy wheel

49
Assignee: CITIC DICASTAL CO LTDPriority: Nov 30, 2017Filed: Nov 13, 2018Published: May 30, 2019
Est. expiryNov 30, 2037(~11.4 yrs left)· nominal 20-yr term from priority
B22C 9/065B22C 9/28B22D 11/055B22D 18/04B22D 27/04
49
PatentIndex Score
0
Cited by
0
References
0
Claims

Abstract

The present application provides a water-cooled mold for casting an aluminum alloy wheel, which is composed of a top mold, a side mold and a bottom mold, wherein a side mold insert is included between the side mold and the bottom mold, the inner surface of the side mold insert faces a cavity, and the upper surface and the lower surface are matched with the side mold frame respectively; the side mold insert is made of copper; the matching surface between the side mold insert and the side mold has a contact matching surface having a length of 10-15 mm at the edges of the inner ring and the outer ring respectively. And the side mold insert and the side mold form a gap which is 0.05-0.20 mm between the contact matching surfaces.

Claims

exact text as granted — not AI-modified
What is claimed is: 
     
         1 . A water-cooled mold for casting an aluminum alloy wheel, comprising a top mold, a side mold and a bottom mold, wherein a side mold insert is arranged between the side mold and the bottom mold, the inner surface of the side mold insert faces a cavity, and the upper surface and the lower surface are matched with the side mold frame respectively; the side mold insert is made of copper; the matching surface between the side mold insert and the side mold has a contact matching surface having a length of 10-15 mm at the edges of the inner ring and the outer ring respectively, and a gap of 0.05-0.20 mm is formed between the side mold insert and the side mold. 
     
     
         2 . The water-cooled mold according to  claim 1 , wherein the matching surface between the side mold insert and the side mold has a contact matching surface having a length of 12 mm at the edges of the inner ring and the outer ring of the matching surface respectively, and a gap of 0.10 mm is formed between the side mold insert and the side mold, and the gap is formed also between the contact matching surfaces. 
     
     
         3 . The water-cooled mold according to  claim 1 , wherein in the water-cooled mold, a cooling water channel of the bottom mold is located on the outer side of the bottom mold.

Cited by (0)

No later patents cite this yet.

References (0)

No backward citations on record.