US2021285164A1PendingUtilityA1

Void reducing asphalt membrane composition, method and apparatus for asphalt paving applications

79
Assignee: HERITAGE RES GROUPPriority: Mar 9, 2015Filed: Dec 22, 2020Published: Sep 16, 2021
Est. expiryMar 9, 2035(~8.7 yrs left)· nominal 20-yr term from priority
C08L 95/00C08K 5/09C08L 93/00C08L 91/06C08L 2205/035E01C 11/24E01C 7/32C08K 2003/2227E01C 11/02C08K 3/013E01C 7/18C08L 23/0838E01C 7/185E01C 7/325E01C 7/30C08L 101/12C08L 53/02C08L 2555/50E01D 11/02C08L 9/06E01C 11/06C08K 3/36C08L 2555/80C08L 2555/60C08L 2555/84C08L 2205/03
79
PatentIndex Score
0
Cited by
0
References
0
Claims

Abstract

A method of sealing pavement joints includes the steps of dispensing a first band of void reducing joint composition on a substrate. Applying a first pass of pavement over at least a portion of the void reducing joint composition. Dispensing a second pass of void reducing joint composition on the substrate. Applying a second pass of pavement of the second band of void reducing joint composition and against an edge of the first pass of pavement.

Claims

exact text as granted — not AI-modified
1 - 11 . (canceled) 
     
     
         12 . A method of forming a pavement construction joint, comprising:
 dispensing a band of a void reducing joint composition on a substrate using at least one spray application vehicle;   permitting the application of a paving pass over the band of joint composition, wherein the paving pass is positioned against an edge of a previously laid portion of pavement to form a pavement construction joint having a volume of air voids; and   allowing at least a portion of the joint composition to migrate upward to reduce the volume of air voids.   
     
     
         13 . The method of  claim 12 , wherein the substrate comprises a pre-existing pavement roadway. 
     
     
         14 . The method of  claim 12 , wherein the void reducing joint composition comprises at least one asphaltic binder, at least one elastomeric polymer, at least one thickener, and at least one additive to reduce tackiness. 
     
     
         15 . The method of  claim 12 , wherein the band of joint composition comprises a thickness of about 1/16 to about ⅜ inch. 
     
     
         16 . The method of  claim 12 , wherein the void reducing joint composition consists essentially of at least one asphaltic binder, at least one elastomeric polymer, at least one thickener, and at least one additive to reduce tackiness. 
     
     
         17 . The method of  claim 16 , wherein the at least one elastomeric polymer comprises a styrene-butadiene-styrene polymer. 
     
     
         18 . The method of  claim 12 , wherein the substrate comprises at least one of an asphalt concrete, a cement concrete, a milled asphalt concrete, a brick surface, or a chip seal surface. 
     
     
         19 . The method of  claim 12 , wherein the substrate comprises a milled asphalt concrete. 
     
     
         20 . The method of  claim 16 , wherein the joint composition comprises about 85 to about 97 wt. % of the least one asphalt binder. 
     
     
         21 . The method of  claim 12 , wherein the joint composition is resistant to lateral flow across the substrate. 
     
     
         22 . The method of  claim 12 , wherein the previously laid portion of pavement is positioned over the band of joint composition. 
     
     
         23 . The method of  claim 12 , wherein the band comprises a width of about 4 to about 24 inches.

Cited by (0)

No later patents cite this yet.

References (0)

No backward citations on record.