Abstract
The present invention provides a one-sided electrode for a secondary battery comprising a current collector, an electrode mixture layer applied to one surface of the current collector, and an electrode distortion-preventing layer formed on the other surface of the current collector to which no electrode mixture is applied. The one-sided electrode according to the present invention exhibits significantly reduced warping or curling after a rolling process and has the advantages of facilitating subsequent processes and enabling enhanced productivity.
Claims
exact text as granted — not AI-modified1 . A one-sided electrode for a secondary battery, comprising:
a current collector; an electrode mixture layer applied on one surface of the current collector; and an electrode distortion-preventing layer formed on another surface of the current collector on which no electrode mixture is applied, wherein the electrode distortion-preventing layer comprises an insulating polymer material.
2 . The one-sided electrode of claim 1 , wherein thickness of the electrode mixture layer is between 1 μm and 70 μm.
3 . The one-sided electrode of claim 1 , wherein a tensile strength of the electrode distortion-preventing layer is 80% to 120% of a tensile strength of the electrode mixture layer,
4 . The one-sided electrode of claim 1 , wherein the insulating polymer comprises one or more selected from the group consisting of polyethylene, polypropylene, polybutylene, polystyrene, polyethylene terephthalate, natural rubber, and synthetic rubber.
5 . The one-sided electrode of claim 1 , wherein the one-sided electrode includes only one current collector.
6 . A secondary battery comprising the one-sided electrode according to claim 1 .
7 . A method of manufacturing the one-sided electrode for the secondary battery according to claim 1 , comprising the steps of:
(a) laminating the electrode distortion-preventing layer on the one surface of the current collector and subsequently applying heat and pressure; (b) applying an electrode active material slurry including an electrode active material and a solvent on the another surface of the current collector; (c) drying the electrode coated with the electrode active material slurry; and (d) rolling the electrode to have a predetermined thickness, wherein the electrode distortion-preventing layer comprises an insulating polymer material.Join the waitlist — get patent alerts