US2023183491A1PendingUtilityA1
Mineral material powder with high dispersion ability and use of said mineral material powder
Est. expiryFeb 17, 2032(~5.6 yrs left)· nominal 20-yr term from priority
Inventors:Pierre BlanchardJean-Pierre ElgoyhenBeat KarthHolger MüllerJürgen SpehnMartin BrunnerPascal GonnonMichael Tinkl
C01P 2006/12D21H 17/675C01P 2006/60D21H 17/67D21H 17/63C04B 14/28D21H 17/66C08K 3/26C01P 2006/22C09C 1/02D21H 19/38C09C 1/021C01P 2004/03D21H 17/68B02C 23/36D21H 19/385C01P 2004/62D21H 17/00C08K 2003/265D21H 21/52D21H 19/40Y02W30/91Y10T428/2982C08K 9/04C09D 1/00Y10T428/2991C09C 3/04
80
PatentIndex Score
0
Cited by
0
References
0
Claims
Abstract
The present invention refers to a mineral matter powder preparation by wet process without acrylic additive or other grinding aid additives and to Me use of said mineral matter after an optional hydrophobic treatment. Said mineral material Having superior dispersing properties.
Claims
exact text as granted — not AI-modified1 - 31 (canceled)
32 . A mineral material obtained by a process comprising the steps of:
a) wet grinding mineral material in at least one grinding step in an aqueous suspension or slurry in the absence of a dispersing agent until the mineral material has a weight median particle diameter d 50 from 0.6 μm to 1.5 μm, wherein the mineral material is selected from the group consisting of marble, chalk, dolomite, calcite, limestone, magnesium hydroxide, talc, gypsum, titanium oxide, and any mixture thereof; b) optionally up-concentrating or dewatering the aqueous suspension or slurry of step a) in the absence of a dispersing agent to achieve a solids content of between 50% and 70%; c) drying the aqueous suspension or slurry of step a) or b) to achieve a solids content of 99.8%, wherein no dispersing agent is present in the mineral material so obtained; d) optionally surface treating the mineral material obtained in step c) with at least one aliphatic carboxylic acid; and e) optionally de-agglomerating the mineral material after step d), wherein the calcium carbonate after grinding in step a) and before optional treatment in step d) has a BET/N 2 specific area of from 3 m 2 /g to 13 m 2 /g, wherein the obtained mineral material has a top cut d 98 from 1.8 μm to 5.9 μm.Join the waitlist — get patent alerts