To provide a cast, hot-worked product of an Al—Mg—Si aluminum alloy which is configured to suppress the development of cracks when a certain tensile load is applied in high humidity, and a method for producing the cast, hot-worked product. A cast, hot-worked product of an Al—Mg—Si aluminum alloy, wherein the aluminum alloy comprises Si and Cu, and wherein an Si/Cu ratio, which is a ratio of a mass % of the Si to a mass % of the Cu, is less than 3.3.
Claims
exact text as granted — not AI-modified1 . A cast, hot-worked product of an Al—Mg—Si aluminum alloy,
wherein the aluminum alloy comprises Si and Cu, and
wherein an Si/Cu ratio, which is a ratio of a mass % of the Si to a mass % of the Cu, is less than 3.3.
2 . A method for producing the cast, hot-worked product of the Al—Mg—Si aluminum alloy defined by claim 1 ,
wherein the method comprises obtaining an ingot by casting the Al—Mg—Si aluminum alloy, and obtaining the cast, hot-worked product by hot-working the ingot, and
wherein a reduction of the cast, hot-worked product in the hot working is 10% or more.
3 . The method for producing the cast, hot-worked product according to claim 2 , wherein the hot working is hot forging.Join the waitlist — get patent alerts