US2025215648A1PendingUtilityA1
Method for coating a paper substrate by using a modified cutin extract
Est. expiryApr 1, 2042(~15.7 yrs left)· nominal 20-yr term from priority
D21H 21/16D21H 17/14D21H 17/02D21H 19/28D21H 19/18D21H 19/20D21H 19/62
58
PatentIndex Score
0
Cited by
0
References
0
Claims
Abstract
The present invention relates to a method for coating a paper substrate comprising: I) providing a paper substrate; ii) applying to the paper substrate an aqueous barrier coating composition having a solids content from 10 to 60 wt % (% by weight) and comprising from 20 to 100 wt % of a modified cutin extract, wherein said modified cutin extract is obtained by thermal treatment of a raw cutin extract at a temperature comprised between 40 and 120° C.
Claims
exact text as granted — not AI-modified1 . A method for coating a paper substrate comprising:
i) providing a paper substrate; ii) applying to the paper substrate an aqueous barrier coating composition having a solids content from 10 to 60 wt % (% by weight) and comprising from 20 to 100 wt % of a modified cutin extract, wherein said modified cutin extract is obtained by thermal treatment of a raw cutin extract at a temperature comprised between 4° and 120° C.
2 . The method for coating a paper substrate according to claim 1 , wherein the aqueous barrier coating composition comprises from 50 to 100 wt % of modified cutin extract.
3 . The method for coating a paper substrate according to claim 1 , wherein the thermal treatment of the raw cutin extract is carried out at a temperature comprised between 6° and 100° C.
4 . The method for coating a paper substrate according to claim 1 , wherein the thermal treatment of the raw cutin extract is carried out at a pH ranging from 2 to 7.
5 . The method for coating a paper substrate according to claim 1 , wherein the thermal treatment of the raw cutin extract is carried out at a pH ranging from 7 to 12.
6 . The method for coating a paper substrate according to claim 1 , wherein the raw cutin extract has a dry content ranging from 30 to 95 wt %.
7 . The method for coating a paper substrate according to claim 1 , wherein the raw cutin extract has a pH ranging from 3 to 6.
8 . The method for coating a paper substrate according to claim 1 , wherein the modified cutin extract has a dry content ranging from 10 to 60 wt %.
9 . The method for coating a paper substrate according to claim 1 , wherein the modified cutin extract has a pH ranging from 6 to 11.
10 . The method for coating a paper substrate according to claim 1 , wherein the aqueous barrier coating composition further comprises pigments, binders, waxes, thickeners, antiblocking agents, dyes, flow control agents or defoamers.Cited by (0)
No later patents cite this yet.
References (0)